Main ingredients: calcium carbonate, cao and additives. Consumption quantity: theory, 1 kilogram "yi" can YGP800 flat meperidine scrape a square meters (two batches). Actual amount for construction method, and different degree of metope. Stir to mix with water of subject construction viscosity, mix, placed 10 minutes (winter placed 30 minutes), then gently. Can't join other materials. Primary treatment should be solid, grass-roots: float ash and dirt, moisture content should be less than 10%. If the grassroots smooth or osteoporosis, need "wall" Gu QG500 interface, wait for dry after appearing to scrape "of YGP800 flat." quack Batch blow be bored with child: due to the high intensity trentment paving, should be bored with child in dry state (with handle gently pressure distortion) using scraper trentment paving, more than 2mm scraping thickness of be bored with child, because each batch of times, scraping thickness should be greater than 0.5 mm (summer), does not exceed 2 mm. A batch of wind thick to dry shrinkage crack. Execution standard: technical standards: JG/T3049-1998 (N), Environmental standards: GB18582-2008. Construction of environment and curing temperature: construction process should be 5 degrees Celsius temperature. Storage and transportation: stored in a cool and dry place, for a period of 12 months. Don't burn, non-toxic products can be stored in accordance with the dangerous goods transport rules. Special remind: due to the paint of alkaline, besmear in grass-roots sensitive to besmear brushs metope paint color twice alkali resistance primer, avoid lacquer, also can improve confirmed the fullness of the film, reduce the consumption of metope lacquer.